PA11 vs PA12, or nylon 11 vs nylon 12 if your supplier uses the older names, is a narrower question than most material comparisons, because on paper the two look almost interchangeable. Same stiffness, same strength, same hardness. If you only read the first three rows of a datasheet you would never pay the premium for PA11.

The difference shows up further down, in impact behaviour, in what happens when the part gets cold, and in where the raw material comes from. Those three things are the entire case for PA11, and on the right part they are decisive.


The Short Answer

PA12 is the default for industrial laser sintering and the right choice for most parts. PA11 is what you specify when the part takes impact, particularly at low temperature, or when a bio-based content figure has to be reported. It costs more, and outside those cases it does not buy you anything PA12 was not already giving you.

Both are polyamides, and the numbers after the PA count carbon atoms in the monomer, which our guide to polyamide vs nylon explains. Both print well, both absorb little moisture compared with PA6 or PA66, and both are stocked as standard sintering grades, PA 860 being the PA11 on our SLS materials list.


Where PA11 Comes From

PA11 is made from a monomer derived from castor oil, which makes it one of the few genuinely bio-based engineering polymers rather than a petrochemical product with a recycled content claim. PA12 is petrochemical in origin.

For a long time that was a marketing footnote. It stopped being one when customers started putting bio-based content into supplier requirements and sustainability reporting, and for some programmes that line in the specification is now the whole reason PA11 is on the drawing. If that applies to you, the material question is already answered and the rest of this comparison is confirmation rather than decision.


The Numbers Side by Side

Both columns below come from EOS datasheets for the two laser sintering grades, measured to ISO methods: the PA 2200 data sheet for PA12 and the PA 1101 data sheet for PA11.

PropertyPA12, EOS PA 2200PA11, EOS PA 1101What it means
Tensile modulus1,700 MPa1,650 MPa in all orientationsEffectively the same stiffness
Tensile strength48 MPa50 MPa in X and Y, 48 MPa in ZEffectively the same strength
Elongation at break24 percent30 percent in X and Y, 15 percent in ZPA11 stretches further before it breaks
Charpy impact, unnotched, 23 CNot stated on the PA 2200 sheet85 kJ per square metre in ZThe headline property
Charpy impact, unnotched, minus 30 CNot stated on the PA 2200 sheet70 kJ per square metre in ZIt keeps most of it in the cold
Charpy notched, 23 CNot stated on the PA 2200 sheet6.9, 7.3 and 5.5 kJ per square metre in X, Y and ZNotches still matter
Shore D hardness7575The same
Density0.93 g per cubic cm1.03 g per cubic cmPA11 is about 11 percent heavier
Melting temperature172 to 180 C201 CPA11 runs hotter

Read the top three rows and the two materials are the same. Modulus differs by about three percent, strength by about four, hardness not at all. Anyone choosing PA11 expecting a stronger or stiffer part has misread what they are buying.

The rows that matter are elongation and impact. PA11 reaches 30 percent elongation against 24 for PA12, and the PA 1101 sheet publishes Charpy impact figures that the PA 2200 sheet does not list at all, including performance at minus 30 degrees C. That is the property you are paying for.

SLS material comparison chart showing Nylon 11, Nylon 12, aluminum filled nylon, glass filled nylon, and flame retarding nylon properties

Impact Is the Real Difference

Elongation at break tells you how far a material stretches before it fails under a steady pull. Impact strength tells you what happens when the load arrives suddenly, and those are different questions. PA11 answers the second one better, which is why it turns up on parts that get dropped, knocked or crashed.

The PA 1101 sheet puts unnotched Charpy impact at 85 kJ per square metre in Z at 23 degrees C. The more interesting number is the one at minus 30 degrees C, which is 70 kJ per square metre. Many polymers become noticeably more brittle as they cool, and a material that keeps most of its impact resistance at minus 30 is telling you something useful about cold service.

Notched values are far lower, at 6.9, 7.3 and 5.5 kJ per square metre in X, Y and Z, and that gap is worth internalising. It means PA11 tolerates a knock on a clean part well, and tolerates a knock on a part with a sharp internal corner much less well. Toughness does not excuse a missing fillet in either material.


Cold Service and Heat

Two temperature facts separate the grades. At the cold end, PA11 holds its impact performance down to at least minus 30 degrees C on the published data, which makes it the sensible default for cold store handling, outdoor equipment and anything that ships or operates in a Canadian winter.

At the hot end, PA11 melts at 201 degrees C against 172 to 180 for PA12. That does not translate directly into a higher service temperature, since service limits depend on load and are better read from heat deflection data, but it does mean more thermal headroom in processing and in brief excursions. If sustained heat resistance is the actual requirement, a glass filled grade addresses it far more directly than switching between unfilled polyamides.

Bridge production run of SLS 3D printed nylon parts on an orange background

What It Costs You

PA11 carries a material premium over PA12, which is the main reason it is not simply the default. We are not going to quote a multiplier here because powder pricing moves and depends on volume, so ask for both prices on your actual part rather than working from a figure in an article.

There is a second cost that is easier to overlook. Density rises from 0.93 to 1.03 grams per cubic centimetre, so an identical part is about 11 percent heavier in PA11. On a handheld product that is nothing. On end-of-arm tooling at full robot reach it is part of the payload budget, and it partly offsets the weight advantage that made a printed tool attractive in the first place.

The practical consequence is the same pattern we apply to filled grades: use the premium material where the property is needed rather than across the whole part. A tough PA11 component mounted into a PA12 structure is usually a better answer than printing everything in PA11.


How to Choose

Choose PA12 unless something specific pushes you off it. It is the industry default for good reasons: it prints predictably, it holds dimension, it costs less, it is lighter, and for the overwhelming majority of tooling and production parts its properties are not the limiting factor.

Choose PA11 when the part takes repeated impact, when it works below freezing, when a living flexure or snap feature needs every bit of ductility available, or when bio-based content is a stated requirement. Those are real cases and in them the premium is easy to justify.

We are Anubis 3D Industrial Solutions. We design and manufacture end-of-arm tooling and produce parts by selective laser sintering in polyamide at our facility in Mississauga, Ontario, and we run both grades. If you are unsure which applies, describe how the part fails rather than what it is made of, because the failure mode usually picks the material for you. Background on the default grade is on our PA12 nylon page.


PA11 and PA12 Questions

What is the difference between PA11 and PA12?

Stiffness, strength and hardness are nearly identical. PA11 has higher elongation at break, 30 percent against 24, better impact resistance including at low temperature, a higher melting point at 201 C against 172 to 180 C, and it is derived from castor oil rather than petrochemicals. It is also denser and more expensive.

Is PA11 stronger than PA12?

No. Tensile strength is 50 MPa against 48, and tensile modulus is actually slightly lower at 1,650 MPa against 1,700. PA11 is tougher rather than stronger, meaning it absorbs impact and stretches further before breaking.

Is PA11 biodegradable?

No. PA11 is bio-based, meaning its monomer is derived from castor oil rather than from petrochemicals, but it is a durable engineering polymer and does not biodegrade. Bio-based content and biodegradability are separate claims and should not be used interchangeably.

When should I choose PA11 over PA12 for 3D printing?

When the part takes impact, especially below freezing, when maximum ductility is needed for a flexing or snapping feature, or when bio-based content is a stated requirement. For most other parts PA12 is lighter, cheaper and perfectly adequate.


Not Sure Which Nylon Your Part Needs?

Tell us how the part fails, where it operates and whether bio-based content is on the specification, and our team will tell you whether PA11 earns its premium on your part or whether PA12 already covers it.


Request a Quote

Tell us what you need and we’ll get back to you with a quote. Pick the one that fits your project.

Let us Stay Connected!

Enjoyed this article? Follow us for more insights, updates, and innovations:

Send Us a Message

This field is for validation purposes and should be left unchanged.
20mb limit. For files larger than that please call us for an FTP link.
Drop files here or
Accepted file types: jpg, png, pdf, stl, step, stp, iges, igs, xt, jpeg, Max. file size: 20 MB.